Due to the expansion of nickel sulfide inclusions (NiS) present within float glass, tempered glass may break without warning. Therefore, heat soak test is highly recommended as it removes more than 95% of the possibility for spontaneous breakage. Please submit specifications and dimensions to request for quotation.
Due to the expansion of nickel sulfide inclusions (NiS) present within float glass, tempered glass may break without warning.

Therefore, heat soak test is highly recommended as it removes more than 95% of the possibility for spontaneous breakage.